Popping

Esquema

Getty AAT: Processes and techniques by specific type

Jerarquía

condition changing processes > surface or structural changes

Descripción

In plaster, the appearance of small, cone-shaped holes up to a quarter inch in diameter; caused by the expansion of lime or foreign material and occurring between three months and up to one year after the plaster has set.

URI original del concepto

http://vocab.getty.edu/aat/300343511

Otros términos

  • popped [en]